Property | Test Method | Typical Performance |
---|---|---|
Tensile strength ( MPa) | ASTM D 2671 | ≥10.4 |
Ultimate elongation ( %) | ASTM D 2671 | ≥ 2 00 |
Tensile strength after heat aged ( MPa ) | 1 58 ℃×168h | ≥7.3 |
Ultimate elongation after heat aged ( % ) | 1 58 ℃×168h | ≥100 |
Longitudinal chang(%) | ASTM D 2671 | -5% ~ +5% |
Flammability | ASTM D 2671 C method | VW-1 |
Voltage withstand | UL 224, 2500V, 60s | No breakdown |
Dielectric strength (kV/mm ) | ASTM D 149 | ≥ 15 |
Volume resistivity (Ω·cm ) | ASTM D 876 | ≥1014 |